Luoyang Hypersolid Metal Tech Co., Ltd

Focusing on customers, market-oriented, constantly innovating, striving for excellence.

Manufacturer from China
Verified Supplier
2 Years
Home / Products / WCu Alloy /

WCu alloy tungsten rod sintered copper tungsten rod tungsten copper alloy rod

Contact Now
Luoyang Hypersolid Metal Tech Co., Ltd
Visit Website
City:luoyang
Country/Region:china
Contact Person:Misssabrina.chen
Contact Now

WCu alloy tungsten rod sintered copper tungsten rod tungsten copper alloy rod

Ask Latest Price
Video Channel
Brand Name :Hypersolid Metal
Place of Origin :China
MOQ :Negotiate
Price :Negitionable
Payment Terms :L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability :10000sets/month
Delivery Time :30 days after receiving down payment
Packaging Details :Standard export cartons
Density :15.63 g/cm3
Electrical Resistivity :≤0.1 μΩ·m
Electricalresistivity :0.22 μΩ·m
Elongation :1-5%
Impactstrength :20 J/cm2
Meltingpoint :1495℃
Tensile Strength :1100-1300 MPa
Yield Strength :>1000MPa
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

1,Description:

Material: WCu alloy is composed of tungsten (W) and copper (Cu) in varying proportions. The most common composition is tungsten content ranging from 70% to 90% by weight, with the remaining percentage being copper.

Density: The density of WCu alloy typically ranges from 14.5 to 16.5 grams per cubic centimeter (g/cm³), depending on the tungsten and copper ratios.

Thermal Conductivity: WCu alloy exhibits a high thermal conductivity due to the presence of copper. The thermal conductivity can range from 180 to 230 watts per meter-kelvin (W/m·K), depending on the specific composition.

2,Specifications:

Property Description
Composition Tungsten (W) and Copper (Cu) alloy
Tungsten Content Typically 70% to 90% by weight
Copper Content Remaining percentage by weight
Density (g/cm³) 14.5 to 16.5
Thermal Conductivity (W/m·K) 180 to 230
Electrical Conductivity 20% to 50% IACS (International Annealed Copper Standard)
Coefficient of Thermal Expansion (CTE) (ppm/°C) 6 to 10
Melting Point (°C) Approximately 3,400
Corrosion Resistance Good resistance to corrosion
Mechanical Strength High mechanical strength